返回
A novel processing method for injection-molded polyether-urethane scaffolds. Part 1: Processing
DOI:10.1002/jbm.b.30396.png)
摘要
En 中文
A large-scale scaffold processing method with injection molding has been successfully developed. Water was used as afoaming agent for the new technique. NaCl was used as a porogen to achieve an open-cell structure. Organic solvents, which are common foaming agents for polyurethane, where not used. Toxic remains in the polymer were therefore prevented. Pore size and porosity was adjustable through process parameters. A parameter study showed that an increase in injection pressure, plasticize speed, cylinder, and mold temperature raised the mean pore diameter. The porosity also could be mended by the cylinder and mold temperature, in addition to NaCl concentration. It was possible to produce scaffolds with a porosity of 64 +/- 3%, a pore size distribution from 30-450 mu m, and a mean pore diameter of 270 +/- 90 mu m. The interconnective pores were found to lie between 5 and 58 mu m. (c) 2005 Wiley Periodicals, Inc.
Keyword:
polyurethane
porous foam
scaffold
crosslinking
crystal growth
DSC (differential scanning calorimetry)
porosity
injection molding
fibroblast
cytotoxicity
AI总结
对已上传原文的论文进行重点信息的提取,主要内容包括:简要概述、研究摘要、背景介绍、关键亮点、图文解析、展望与总结。
期刊
IF:
3.4
论文数:
5.1K
被引数:
1.1W
机构
暂无机构信息
引用论文
Novel approach to fabricate porous sponges of poly(D,L-lactic-co-glycolic acid) without the use of organic solvents
BIOMATERIALS
IF12.9
Citations and thehindex of soil researchers and journals in the Web of Science, Scopus, and Google Scholar
PeerJ
IF0
Supercritical carbon dioxide aided preparation of conductive polyurethane-polypyrrole composites超临界二氧化碳辅助制备导电聚氨酯-聚吡咯复合材料