The Faraday Discussion on Photoelectron Spectroscopy and the Future of Surface Analysis was held both in person and virtually in London, April 20-22, 2022. In my concluding lecture I have highlighted three different recent directions in the field; (i) in situ and operando, (ii) buried interfaces and (iii) time resolved measurements. I have based my lecture on most recent studies conducted in my research group in all these 3 directions. In particular, the new operando instrument POLARIS, located at the brightest hard X-ray beamline at DESY for photoelectron spectroscopy, has opened new avenues to address important problems in catalysis that are essential for society to become fossil free.
Keywords:
CO OXIDATION
METHANOL SYNTHESIS
REDUCTION
CATALYSTS
SELECTIVITY
ELECTRODES
INDUSTRIAL
ENERGIES
STATE

Journal

Faraday Discussions cover
Faraday Discussions
IF:
3.1
Papers:
4.4K
Citations:
1.0W

Organization

S
Stockholm University
Scholars:
1.8W
Papers: 1.7W
Citations: 30
Cited Papers

Cited Papers

Citing Papers

Citing Papers