Abstract

Abstract

En 中文
Compressive creep tests were performed on a CoCrFeNiMn equiatomic alloy with the dispersion of (i) aluminum nitride or (ii) boron nitride at temperatures of 973 K and 1073 K. The results are compared with previously published creep rates of the unreinforced matrix alloy and the alloy when strengthened by yttrium + titanium oxides. The comparison reveals that the creep rate is essentially unchanged by the presence of aluminum nitride particles, whereas it is reduced by the presence of oxide particles. Boron nitride particles do not influence the creep rate at low stresses but reduce it substantially at high stresses.
Keywords:
creep
high-entropy alloy
dispersion-strengthened alloy
spark plasma sintering

Journal

Materials cover
Materials
IF:
3.2
Papers:
5.6W
Citations:
15.1W

Organization

C
czech academy of sciences
Scholars:
3.4W
Papers: 2.6W
Citations: 31
Cited Papers

Cited Papers

Citing Papers

Citing Papers