Does microstructure matter for statistical nanoindentation techniques?

delete2010-01-01
delete147
PRE
AI
F
Franz‐Josef Ulm *
M
Matthieu Vandamme
H
Hamlin M. Jennings
J
J. Vanzo
M
Michelle Bentivegna
K
Konrad J. Krakowiak
G
Georgios Constantinides
C
Christopher P. Bobko
K
Krystyn J. Van Vliet
DOI:10.1016/j.cemconcomp.2009.08.007delete
delete原文链接
delete原文求助
delete分享
delete收藏
摘要

摘要

En 中文
In their paper, Trtik et al. (2009) identify spurious peaks in the application of statistical nanoindentation technique as a critical obstacle for mechanical phase identification. In this discussion. we show that Trtik et al.'s finding is a consequence of an unrealistic virtual 3-D checkerboard microstructure considered by the authors. These peaks are not a general feature of indentation on multiphase materials, nor can the presence of such peaks be attributed to an intrinsic shortcoming of the grid-indentation technique. We also show that the authors' assertion of the absence of homogeneous material regions extending beyond 3 pm in cementitious materials is groundless. (C) 2009 Elsevier Ltd. All rights reserved.
Keyword:
Nanoindentation
Statistical analysis
Microstructure
AI总结

AI总结

对已上传原文的论文进行重点信息的提取,主要内容包括:简要概述、研究摘要、背景介绍、关键亮点、图文解析、展望与总结。

期刊

Cement and Concrete Composites 封面图
Cement and Concrete Composites
IF:
13.1
论文数:
5.4K
被引数:
5.1W

机构

U
universidade do minho
学者数:
1.1W
论文数: 1.1W
被引数: 10
C
Cyprus University of Technology
学者数:
2.1K
论文数: 2.1K
被引数: 2.6K
E
ecole des ponts paristech
学者数:
1.2K
论文数: 989
被引数: 1
I
institut polytechnique de paris
学者数:
1.3W
论文数: 1.0W
被引数: 6
N
Northwestern University
学者数:
6.2W
论文数: 5.3W
被引数: 3.9K
学者 查看更多机构
引用论文

引用论文

The nano-mechanical morphology of shale
err2008-04-01
err220
PREAI
errBobko, Christopher; Ulm, Franz-Josef
err分享
err收藏
Statistical indentation techniques for hydrated nanocomposites: Concrete, bone, and shale
err2007-09-05
err511
errOAAI
errUlm, Franz-Josef; Vandamme, Matthieu; Bobko, Chris; Ortega, Jose Alberto
err分享
err收藏
err分享
err收藏
A multi-technique investigation of the nanoporosity of cement paste
err2007-03-01
err386
errOAAI
errJennings, Hamlin M.; Thomas, Jeffrey J.; Gevrenov, Julia S.; Constantinides, Georgios; Ulm, Franz-Josef
err分享
err收藏
Composition and density of nanoscale calcium-silicate-hydrate in cement
err2007-03-25
err875
PREAI
errAllen, Andrew J.; Thomas, Jeffrey J.; Jennings, Hamlin M.
err分享
err收藏
err分享
err收藏
学者 查看更多内容