Improving atomic layer deposition process through reactor scale simulation

delete2014-11-01
delete25
PRE
AI
M
Mohammad Reza Shaeri
T
Tien‐Chien Jen *
C
Chris Yuan
DOI:10.1016/j.ijheatmasstransfer.2014.07.079delete
delete原文链接
delete原文求助
delete分享
delete收藏
摘要

摘要

En 中文
In order to modify atomic layer deposition (ALD) characteristics of Al2O3, three-dimensional gas transports and film depositions are investigated through reactor scale simulations inside two different viscous flow reactors. In the top-inlet reactor (TIR), the gaseous species are directly injected into the substrates from the upper surface of the reactor while in the bottom-inlet reactor (BIR), the inlet is at the bottom of the reactor and next to the substrate. The numerical procedure to simulate the ALD process is thoroughly explained by using the multi-species and multi-reaction chemistry phenomena. The reactants are trimethylaluminum (TMA) and ozone, and the simulations are performed in an operating pressure of 10 Tort (1330 Pa) and two substrate temperatures of 250 degrees C and 300 degrees C. Due to the chemistry mechanism used in this study, a long ozone exposure is a crucial parameter to deliver a sufficiently oxidized substrate. For a specific reactor type, deposition rates are higher on the hotter substrate due to both a larger surface reaction rate constant and greater concentrations of the oxygen atoms on the substrate. At a fixed substrate temperature, higher deposition rates are obtained by using the TIR. The same deposition rate distributions are obtained among all cycles for each ALD process that result in the dependency of the film thickness only on the numbers of ALD cycles. For the substrate at 250 degrees C, the growth rates are equal to 3.78 angstrom/cycle and 4.43 angstrom/cycle in the BIR and the TIR, respectively, and for the substrate at 300 degrees C, the growth rates are equal to 4.52 angstrom/cycle and 6.49 angstrom/cycle in the BIR and the TIR, respectively. (C) 2014 Elsevier Ltd. All rights reserved.
Keyword:
Atomic layer deposition
Gas-phase reaction
Surface reaction
Navier-Stokes equation
Viscous flow reactor
Mass deposition rate
AI总结

AI总结

对已上传原文的论文进行重点信息的提取,主要内容包括:简要概述、研究摘要、背景介绍、关键亮点、图文解析、展望与总结。

期刊

International Journal of Heat and Mass Transfer 封面图
International Journal of Heat and Mass Transfer
IF:
5.8
论文数:
2.6W
被引数:
10.2W

机构

University of Wisconsin System 封面图
University of Wisconsin System
学者数:
6.7W
论文数: 5.8W
被引数: 382
引用论文

引用论文

Building Trust in the Human?Internet of Things Relationship
err2014-01-01
err0
PREAI
errIoannis Kounelis; Gianmarco Baldini; Ricardo Neisse; Gary Steri; Mariachiara Tallacchini; Angela Guimaraes Pereira
err分享
err收藏
Genetic variation in C57BL/6 ES cell lines and genetic instability in the Bruce4 C57BL/6 ES cell line
err2007-09-09
err0
PREAI
errElizabeth D. Hughes; Yun Yan Qu; Suzanne J. Genik; Robert H. Lyons; Christopher D. Pacheco; Andrew P. Lieberman; Linda C. Samuelson; Igor O. Nasonkin; Sally A. Camper; Margaret L. Van Keuren; Thomas L. Saunders
err分享
err收藏
Numerical investigation of conductance of porous media in high vacuum systems
errVACUUM
IF3.9
err2011-10-01
err6
PREAI
errGharamaleki, Yunes Shafaat; Shams, Mehrzad
err分享
err收藏
Measurement of conductance of a sapphire sealed variable leak valve
errVACUUM
IF3.9
err2013-12-01
err6
PREAI
errAvdiaj, Sefer; Setina, Janez; Erjavec, Bojan
err分享
err收藏
On the influence of vacuum on the design and characterization of MEMS真空对MEMS设计和表征的影响
errVACUUM
IF3.9
err2012-01-01
err19
PREAI
errDienel, Marco; Naumann, Michael; Sorger, Alexander; Tenholte, Dirk; Voigt, Sebastian; Mehner, Jan
err分享
err收藏
学者 查看更多内容