Improving the stress corrosion cracking resistance of ultra-high strength engineering marine steel by binary method regulation

delete2026-07-24
delete0
PRE
AI
G
Guangming Yang
L
Lili Zhang
X
Xuexu Xu
W
Weibing Wang *
H
Hongchi Ma
刘智勇 (Zhiyong Liu) *
X
Xiaolin Li
DOI:10.1016/j.corsci.2026.114135delete
deleteOriginal
deleteOriginal request for help
deleteShare
deleteSave
Abstract

Abstract

En 中文
• A binary method is proposed to improve the SCC resistance of marine engineering steel. • Anti-AD mechanism originates from the coupling of microstructural optimization and a compact composite rust layer. • Anti-HE mechanism arises from surface barrier inhibiting hydrogen absorption and bulk multiscale hydrogen trapping.

Journal

Corrosion Science cover
Corrosion Science
IF:
8.5
Papers:
1.3W
Citations:
7.3W

Organization

C
china university of petroleum
Scholars:
4.0W
Papers: 2.7W
Citations: 30
U
university of science and technology beijing
Scholars:
1.1W
Papers: 4.0K
Citations: 2
C
city university of hong kong
Scholars:
4.6K
Papers: 2.7K
Citations: 2
Cited Papers

Cited Papers

Citing Papers

Citing Papers