Stabilizing Nanostructured Solid Oxide Fuel Cell Cathode with Atomic Layer Deposition
DOI:10.1021/nl402138w.png)
摘要
En 中文
We demonstrate that the highly active but unstable nanostructured intermediate-temperature solid oxide fuel cell cathode, La0.6Sr0.4CoO3-delta (LSCo), can retain its high oxygen reduction reaction (ORR) activity with exceptional stability for 4000 h at 700 degrees C by overcoating its surfaces with a conformal layer of nanoscale ZrO2 films through atomic layer deposition (ALD). The benefits from the presence of the nanoscale ALD-ZrO2 overcoats are remarkable: a factor of 19 and 18 reduction in polarization area-specific resistance and degradation rate over the pristine sample, respectively. The unique multifunctionality of the ALD-derived nanoscaled ZrO2 overcoats, that is, possessing porosity for O-2 access to LSCo, conducting both electrons and oxide-ions, confining thermal growth of LSCo nanoparticles, and suppressing surface Sr-segregation is deemed the key enabler for the observed stable and active nanostructured cathode.
Keyword:
Solid oxide fuel cell
atomic layer deposition
cathode
degradation
期刊
IF:
9.1
论文数:
2.7W
被引数:
16.5W
机构
引用论文
Electrochemical performance and degradation of (La0.6Sr0.4)0.99CoO3-δ as porous SOFC-cathode
SOLID STATE IONICS
IF3.3
Time-dependent performance changes in LSCF-infiltrated SOFC cathodes: The role of nano-particle coarseningLSCF渗透的SOFC阴极随时间变化的性能变化: 纳米颗粒粗化的作用
SOLID STATE IONICS
IF3.3