Return
Distinct orientation dependence of plasticity initiation and subsequent deformation in nanoindented tungsten
F
T
DOI:10.1016/j.ijrmhm.2026.107907.png)
Abstract
En 中文
• Clear orientation dependence for indent appearance, pop-in stress and hardness. • Highest hardness of 5.18 ± 0.07 GPa and lowest pop-in stress on {100} surface. • On {111} surface grooves formed in agreement with pronounced slip. • Non-Schmid stresses may contribute to long 〈111〉 glide parallel to {110} surface.
Keywords:
Nanoindentation
Tungsten
Orientation-dependence
Yield phenomena
Plastic deformation
AI Summary
Key information extracted from the uploaded paper, including a brief overview, abstract, background, key highlights, visual analysis, and future outlook.
Journal
IF:
4.6
Papers:
5.3K
Citations:
1.4W