Fractography—Microscopic Cracking Processes
DOI:10.1520/stp600-eb.png)
Abstract
En 中文
Description
The Symposium on Fractograph—Microscopic Cracking Processes was held at the Seventy-eighth Annual Meeting of the American Society for Testing and Materials held in Montreal, Canada, 22-27 June 1975. ASTM Commitee E24 on Fracture Testing of Metals sponsored the symposium. C. D. Beachem, Naval Research Laboratory, and W. R. Warke, Illinois Institute of Technology, served as symposium cochairmen.