Pressureless sintering of ultra-low-binder WC-Ni Hardmetals via bimodal powder packing and colloidal processing
A
B
E
A
S
J
A
DOI:10.1016/j.ijrmhm.2026.107925.png)
Abstract
En 中文
• Pressureless sintering yields >97% density in WC-Ni hardmetals with 1 vol-% Ni. • Bimodal packing efficiency is maximized at 25–30 vol-% total submicron fraction. • Sintering is accelerated by n-WC, while Ni content defines densification pathways. • XRD and HR-TEM reveal an η-carbide (Ni₂W₄C) interphase between WC and Ni.
Keywords:
Particle packing
Pressureless sintering
Hardmetals
WC-Ni
Nanosized WC